1st dilute A c with 2parts water let sit so clorine evaporats
2nd use supersatured solution of sodiummetabisulfite (smb)
3rd add smb to auric chloride a little at a time and let stand as gold oxide presipatates out of solution
now the brown at the bottom is gold oxide
next amalgamate with borax and lots of heat
voala shyknee gold stuff